首页> 外文会议>Photonics and optoelectronics meetings >Laser damage performance of large-aperture fused silica opticalcomponents at 351 nm
【24h】

Laser damage performance of large-aperture fused silica opticalcomponents at 351 nm

机译:351 nm的大光圈熔融二氧化硅光学组分的激光损伤性能

获取原文

摘要

High power laser facility for ICF will routinely operate at high fluence level. The damage on the large-area FOA opticsis a key lifetime limiter. The optics should be checked after each laser shot for damage initiation and growth. On-linemonitoring equipments are installed for this purpose. Damage pictures of a fused silica component are successfully takenand the luminance of the pictures could reflect the deterioration of the operational environment .Damage initiation andgrowth behaviors at 351nm high-fluence laser were observed. Damage density and damage growth are exponential withthe shot number and some conclusions could be drawn. These results bring forward demands for future monitoringequipments and more experiments to establish a lifetime model.
机译:对ICF的高功率激光设施将在高流量水平下经常运行。大面积FOA OPTICSIS损坏关键寿命限制器。每个激光射击后应检查光学器件是否损坏启动和生长。为此目的安装了在线设备设备。损坏熔融二氧化硅组分的图片成功地占据了图片的亮度,可以反映操作环境的恶化。观察到351nm高流速激光的阳光发育和生长行为。损伤密度和损伤的增长是指数级,射门数量和一些结论可以绘制。这些结果提出了未来监控方案的要求和更多实验建立终身模型。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号