Nano-crystallite preparation by pulsed-laser induced reaction at liquid-solid interface

机译:纳米微晶通过脉冲激光诱导反应在液固界面反应制备

获取原文

摘要

A novel method, pulsed-laser induced reaction at liquid-solid interface (PLIIR), which is used to synthesize nanostallite, is developed. Nano-crystalline diamond with hexagonal lattice and cubic lattice and carbon nitride, which phasesdudeα-C{sub}3N{sub}4, graphite-C{sub}3N{sub}4, β-C{sub}3N{sub}4 and cubic-C{sub}3N{sub}4, are synthesized by this approach. Trans-mission electron microscopy(TEM), high resolution electron micro-scopy(HREM) and other methods are used to characterize the structures the nano-crystallite. Graphite-C{sub}3N{sub}4 and cubic-C{sub}3N{sub}4 are reported for the first time in experiment.
机译:一种新的方法,脉冲激光诱导在液体固体界面(PlIIR)中的反应,其用于合成纳米烷基钛矿。纳米结晶金刚石与六边形格子和立方晶格和碳氮化物,哪个阶段Dudeα-C {Sub} 4,Graphite-C {Sub} 3N {Sub} 4,β-C {Sub} 3N {Sub} 4通过这种方法合成三次-C {sub} 3n {sub} 4。反式任务电子显微镜(TEM),高分辨率电子微型SCOPY(HREM)和其他方法用于表征纳米微晶的结构。在实验中首次报告Graphite-C {Sub} 3N {sub} 4和立方-c {sub} 4。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号