Despite the several benefits of modifying bitumen with polymer; it is increasingly becoming difficult to ignore concerns about its high energy consumption and fume emissions during asphalt production. Previous studies found on natural rubber (NR) modified binders applied it as a hot mix asphalt (HMA), however in recent years there has been increasing interest in warm mix asphalt. This research explores the possibility of applying NR in warm mix asphalt (WMA) by comparing the physical properties of cup lump rubber modified bitumen with and without warm mix additive. Four percentages (2.5%, 5.0%, 7.5% and 10%) of Cup lump rubber (CLR) was used to modify 60/70 penetration grade bitumen, while three percentages (0.3%, 0.4%, and 0.5%) of Evotherm chemical was added to produce warm cup lump modified bitumen (WCMB). Storage stability, penetration, softening point, viscosity, ductility, and elastic recovery tests were conducted to determine the effect of CLR and Evotherm. The results show that storage stability and viscosity of the cup lump modified bitumen heavily depends on the CLR content. While a positive correlation exists between the increase in binder stiffness with increasing mixing and compaction temperatures. The addition of 0.5% Evotherm reduces the viscosity by 14%. Contrary to expectations, CLR was found to reduce the ductility of the bitumen while the presence of Evotherm in the blend increases the softening point. The use of warm NR modified bitumen in road construction is expected to lower the asphalt production temperature, carbon emission and cost without compromising the performance of the mix.
机译:尽管用聚合物改性沥青的几个好处;甚至难以忽视其在沥青生产中对其高能量消耗和烟雾排放的担忧。在天然橡胶(NR)修饰的粘合剂上发现的先前研究将其作为热混合物沥青(HMA)施加,然而近年来对温热沥青的兴趣越来越令人感兴趣。本研究探讨了通过比较杯块橡胶改性沥青的物理性质在具有和不具有温热的添加剂的情况下施加湿混沥青(WMA)中施加NR的可能性。四个百分比(2.5%,5.0%,7.5%和10%)的杯块橡胶(CLR)用于修饰60/70渗透级沥青,而三个百分比(0.3%,0.4%和0.5%)的Evotherm Chemical加入生产温杯块改性沥青(WCMB)。进行储存稳定性,渗透,软化点,粘度,延展性和弹性恢复试验,以确定CLR和EVOTHERM的效果。结果表明,杯块改性沥青的储存稳定性和粘度大大取决于CLR含量。虽然在粘合剂刚度的增加与增加混合和压实温度之间存在正相关性。加入0.5%Evotherm将粘度降低14%。与期望相反,发现CLR降低沥青的延展性,而混合物中的Evotherm的存在增加了软化点。预计在道路结构中使用温暖的NR改性沥青将降低沥青生产温度,碳排放和成本,而不会影响混合物的性能。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号