UTILIZATION OF PALM OIL AND ELECTRIC POWER PLANT FLY ASH WASTE MATERIAL AS A CLAY REPLACEMENT IN BRICKS

机译:棕榈油和电力厂粉煤灰废料的利用用作砖块的粘土替代品

获取原文

摘要

In this study bricks samples were produced containing substituent from palm oil and electric power plant fly ash. These waste products are used to replace the natural ingredient in the manufacturing of brick clay namely as clay. At the present, the world's natural resources are decreasing so many alternative actively pursued to ensure that the natural ingredients will remain unchanged for the use of the more significant and worthwhile. In this study, some suggestions have been proposed where the using of fly ash as a clay replacement materials in the percentage of 20%, 40% and 60%. The several laboratory experiments was carried out, where the high compressive strength with 20% of fly ash replacement is 15.5 N/mm~2 while for the 20% of power plant fly ash replacement provide a compressive strength of 103 N/mm~2. For optimum water absorption, the rate is 17.05% which is from 20% of palm oil fly ash replacement while for brick from 60% power plant fly ash, the rate of water absorption is 4.96%. Therefore, this study can contribute to recycling the industrial waste material as a replacement material in brick in Malaysia.
机译:在该研究中,砖样品含有棕榈油和电力厂飞灰的取代基。这些废物产品用于取代砖块制造中的天然成分,即粘土。目前,世界的自然资源正在减少这么多的替代方案,以确保使用更重要和有价值的自然成分保持不变。在这项研究中,提出了一些建议,其中粉煤灰作为粘土替代材料的百分比为20%,40%和60%。进行了几个实验室实验,其中具有20%的飞灰更换的高压缩强度为15.5 n / mm〜2,而20%的电厂粉煤灰更换提供103n / mm〜2的抗压强度。为了获得最佳吸水性,速率为17.05%,为棕榈油粉煤灰的20%,而从60%发电厂粉煤灰的砖块,吸水率为4.96%。因此,该研究可以有助于将工业废料作为马来西亚砖中的替代材料回收。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号