A Ti-47AI-2Cr-2Nb (at.%) material was fabricated using two laser-based methods, "Selective Laser Melting" (SLM) and "Direct Metal Deposition" (DMD), for potential uses in aircraft jet engines. Experiments were conducted under controlled atmosphere by changing the processing param Optimal parameters were searched for this relatively low ductility material to prevent cracking due to built-up residual stresses during fast cooling. It was observed that these non-equilibrium cooling conditions were fast enoughtto generate ultra fine 'and metastable structures exhibiting high microhardness values. Post heat-treatments were successfully used to restore homogeneous lamellar or duplex microstructures and to relieve the residual stresses. A comparison of these two methods' is provided in terms of powder requirements and of process parameters to achieve noncracked structures and fully dense materials.
机译:使用两种基于激光的方法,“选择性激光熔化”(SLM)和“直接金属沉积”(DMD)制造Ti-47ai-2Cr-2NB(AT.%)材料,用于飞机喷射发动机的潜在用途。通过改变对受控气氛进行实验,通过改变处理参数最佳参数,以防止由于在快速冷却期间由于内置残余应力而导致的裂缝。观察到这些非平衡的冷却条件是快速产生的超细'和亚稳结构,呈现出高度微硬度值。后热处理成功用于恢复均匀的层状层或双工微结构并缓解残余应力。这两种方法的比较是在粉末要求和工艺参数方面提供的,以实现非折叠结构和完全致密的材料。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号