Corrosion rates at the top and bottom of the pipe have been measured in wet gas multiphase flow at carbon dioxide partial pressures of 0.46 MPa and temperatures of 40 C and 60 C in a high pressure 10-cm diameter system.Gas velocities up to 30 m/s and liquid velocities up to 0.5 m/s were used.The liquid consisted of a mixture of de-ionized water and low viscosity oil at two water cuts of 80% and 40%,and carbon dioxide was used in the gas phase.Corrosion inhibition studies were carried out at 50 ppm and 100 ppm dosage levels.The inhibitor used was an oleic imidazoline active compound dissolved in isopropyl alcohol and water.
机译:管道顶部和底部的腐蚀速率已经在0.46MPa的二氧化碳部分压力下的湿气体多相流动下测量,在高压10-cm直径的高压10-cm和60℃的温度下。总速度高达30米使用高达0.5m / s的液体速度。液体由脱离离子水和低粘度油的混合物,在80%和40%的两个水中,并且在气相中使用二氧化碳。腐蚀抑制研究以50ppm和100ppm剂量水平进行。所用的抑制剂是溶于异丙醇和水中的油酸咪唑啉活性化合物。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号