Fireside Corrosion in Coal-and Oil-Fired Units:Failure Mechanisms and Methods of Prevention

机译:燃煤装置中的壁式腐蚀:预防机制和预防方法

获取原文

摘要

Fireside corrosion shortens the service life of tubes in coal-fired and oil-fired boilers.Waterwall and superheater/reheater tubes may experience substantial wall loss as a result of fireside corrosion.Waterwall tube failures due to fierside corrosion are less common than failure of superheater/reheater tubes.Therefore,comments respective to waterwall tube failures are addressed only in the introduction section of this paper.Mechanisms of failures involving fireside corrosion of superheaters/reheaters are presented as Case Studies using actual laboratory analysis data.Available approaches to minimize fireside corrosion of superheaters/reheaters are reviewed.
机译:炉边腐蚀缩短了燃煤和燃油锅炉中管的使用寿命。水坑和过热器/再热器管可能由于壁式腐蚀而经历了大量的墙壁损失。由于Fierside腐蚀引起的水管管失效不太常见于过热器失效因此,只有在本文的介绍部分中,对水坑管故障的评论仅在本文的介绍部分中解决了涉及过热剂/再美分的故障的故障机制作为使用实际实验室分析数据的案例研究。可利用的方法,以最大限度地减少壁式腐蚀的方法综述超热/再次审查。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号