摘要

Increase of the energy recovery efficiency facilities is one of the challenges fixed recently by UE to Municipal Solid Waste Incineration (MSWI) operators. To achieve this target, one option consists in optimizing the water/steam cycle to increase electrical efficiency. Nevertheless, higher steam temperature into heat exchanger tube is expected to increase the risks of fireside corrosion, particularly on superheater tubes, along with important loss of materials, frequent shutdowns for repairs and high operational costs. In this study, fireside corrosion test had been performed using an innovative laboratory-scale corrosion pilot. Effect of increase in metal temperature from 400℃ to 450℃ on corrosion performances of SA192 carbon steel tube and AISI 316L stainless steel had been examined. Mechanisms and corrosion rates are discussed with regards to lifetime reported for both materials after 1 year in service in the same plant.
机译:能源回收效率设施的增加是UE最近解决的市政固体废物焚化(MSWI)运营商面临的挑战之一。为了实现这一目标,一种选择是优化水/蒸汽循环以提高电效率。然而,进入换热器管的蒸汽温度较高,预计会增加炉侧腐蚀的风险,特别是在过热器管上,同时还会损失大量材料,频繁停工进行维修以及较高的运营成本。在这项研究中,使用创新的实验室规模的腐蚀试点进行了炉边腐蚀测试。研究了金属温度从400℃升高到450℃对SA192碳钢管和AISI 316L不锈钢腐蚀性能的影响。讨论了有关两种材料在同一工厂使用一年后报告的使用寿命的机理和腐蚀速率。

著录项

  • 来源
    《Materials science forum》 |2011年第2011期|p.212-217|共6页
  • 作者单位

    Veolia Environnement Research and Innovation, 291 Avenue Dreyfous Ducas, Limay, France;

    Veolia Environnement Research and Innovation, 291 Avenue Dreyfous Ducas, Limay, France;

    Veolia Environnement Research and Innovation, 291 Avenue Dreyfous Ducas, Limay, France;

    Institut Jean Lamour, UMR 7198 CNRS - Universite Henri Poincare Nancy 1,Vandceuvre-Les-Nancy, France;

    Institut Jean Lamour, UMR 7198 CNRS - Universite Henri Poincare Nancy 1,Vandceuvre-Les-Nancy, France;

  • 收录信息
  • 原文格式 PDF
  • 正文语种 eng
  • 中图分类
  • 关键词

    fireside corrosion; waste-to-energy; aisi 316l;

    机译:炉边腐蚀;浪费能源;爱思316l;

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号