The coupling process of sphalerite concentrate leaching in FeCl3-HCl solutions and tetrachloroethylene extracting of sulfur were studied. Principle of leaching and effects of leaching temperature, leaching time and tetrachloroethylene concentration on leaching processes were investigated separately. The results indicated that 96.7% zinc extraction was obtained after four hours of leaching at 85 °C, with 10g sphalerite concentrate in 200ml solution containing 3.0 mol/L FeCl3, 2.0 mol/L HC1 and 0.2 g/L surfactant, in the presence of 10 ml tetrachloroethylene. The zinc extraction was 20% higher than the common leaching. The coupling effect was distinct.
机译:研究了Sphalerite浓缩物浸出的偶联方法在FECL 3 -HCL溶液中和四氯乙烯萃取硫。分别研究了浸出温度,浸出时间和四氯乙烯浓度对浸出过程的浸出和浸出方法的原理。结果表明,在85℃下浸出四小时后,得到96.7%的锌提取,其中含有3.0mol / L FeCl 3 ,2.0mol / L HC1和0.2g / L表面活性剂,在10ml四氯乙烯存在下。锌提取比常见的浸出量高20%。偶联效果明显。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号