The sintering behavior and microwave dielectric properties of the (Ca_(0.9375)Sr_(0.0625))_(0.25)(Li_(0.5)Sm_(0.5))_(0.75)TiO_3 (CSLST) ceramics doped with different amounts of Li_2O-B_2O_3-SiO_2-CaO-Al_2O_3(LBSCA) glass were investigated. The sintering temperature of the CSLST ceramics can be effectively reduced over 200"C due to the addition of LBSCA glass. For the 5 wt% LBSCA-doped CSLST ceramics, which are sintered at only 1000°C for 5 h, show optimum microwave dielectric properties as follows: ε_r=84.74,Qf=2446 GHz and τ_f=-12.48 ppm/°C.
机译:掺杂不同量Li_2O-B_2O_3的(Ca_(0.9375)Sr_(0.0625))_(0.25)(Li_(0.5)Sm_(0.5))_(0.75)TiO_3(CSLST)陶瓷的烧结行为和微波介电性能研究了-SiO_2-CaO-Al_2O_3(LBSCA)玻璃。通过添加LBSCA玻璃,可以有效地将CSLST陶瓷的烧结温度降低到200“ C以上。对于仅在1000°C烧结5 h的5%LBSCA掺杂的CSLST陶瓷,其微波介电性能最佳特性如下:ε_r= 84.74,Qf = 2446 GHz和τ_f= -12.48 ppm /°C。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号