首页> 外文会议>TMS(The Minerals, Metals Materials Society) Annual Meeting >AN IMPROVED RAYLEIGH NUMBER CRITERION FOR FRECKLE PREDICTION INCORPORATING THE EFFECT OF CARBIDES
【24h】

AN IMPROVED RAYLEIGH NUMBER CRITERION FOR FRECKLE PREDICTION INCORPORATING THE EFFECT OF CARBIDES

机译:结合了碳化物效果的改进的弗雷格数准则

获取原文
获取外文期刊封面目录资料

摘要

Freckle chains are lines of equiaxed grains which may form during the directional solidification of single crystal Ni-base superalloys. In single crystal alloys freckles form as a result of convective flow of the lighter interdendritic liquid that tends to flow upward towards the heavier bulk composition liquid. Both the interdendritic liquid density and the permeability of the mushy zone affect freckle formation. The Rayleigh number, which is the ratio of the buoyancy to the drag forces in the liquid, is used to assess the likelihood of freckle occurrence. The addition of carbon has been shown to significantly reduce the number of solidification defects, including freckles. The formation of carbides in the interdendritic region will influence both the effective density of the fluid and the structure's permeability. Using a combination of mesoscale solidification modeling and thermodynamic calculations, these two effects were incorporated into an improved Rayleigh number criterion and compared to experimentally observed freckles as a function of the carbon content.
机译:雀斑链是等轴晶粒的线,它们可能在单晶镍基高温合金的定向凝固过程中形成。在单晶合金中,由于较轻的树枝状液体的对流流动而形成了雀斑,该对流倾向于向上流向较重的本体组合物液体。树突间的液体密度和糊状区的渗透性都会影响雀斑的形成。瑞利数是液体中浮力与阻力的比值,用于评估出现雀斑的可能性。碳的添加已显示可显着减少凝固缺陷(包括雀斑)的数量。枝晶间区域中碳化物的形成将影响流体的有效密度和结构的渗透性。结合使用中尺度凝固模型和热力学计算,将这两种作用结合到改进的瑞利数准则中,并与实验观察到的雀斑作为碳含量的函数进行了比较。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号