The Effects of Different Hydroxyapatite/TiO2 Composite Coatings on Protein Expression of Osteoblast

机译:不同羟基磷灰石/ TiO2复合涂层对成骨细胞蛋白质表达的影响

获取原文

摘要

Hydroxyapatite/TiO2 composite material was coated onto Ti25Nb3Mo2Sn3Zr (TLM) alloy substrate. To study the effects of hydroxyapatite/TiO2 composite coatings on bone-related protein expression, the osteoblast were cultured with composite coatings for different times. The phase transformation and compound formation of the HA/TiO2 coatings were investigated using XRD (X-ray diffraction). The mRNA expression of Type I collagen, alkaline phosphatase (ALP) and osteocalcin were studied by RT-PCR (reverse transcriptional polymerase chain reaction). The titania delayed the crystallization of HA. The mRNA expressions of Type I collagen are decreased as the increasing of TiO2 percentage. The mRNA expressions of osteocalcin are approached. The ALP expression on H4 coating (HA/TiO2 mol ration is 5) after the osteoblast cultured with composite coating for 6 days is the highest. The increasing of TiO2 amount decreases the bioactivity of the composite coatings.
机译:将羟基磷灰石/ TiO2复合材料涂覆到Ti25Nb3Mo2Sn3Zr(TLM)合金基底上。为了研究羟基磷灰石/ TiO 2复合涂层对骨相关蛋白表达的影响,将成骨细胞与复合涂层一起培养不同的时间。使用XRD(X射线衍射)研究了HA / TiO2涂层的相变和化合物形成。通过RT-PCR(逆转录聚合酶链反应)研究了I型胶原,碱性磷酸酶(ALP)和骨钙素的mRNA表达。二氧化钛延迟了HA的结晶。 I型胶原的mRNA表达随TiO2百分比的增加而降低。接近骨钙素的mRNA表达。成骨细胞复合涂层培养6天后,H4涂层(HA / TiO2摩尔比为5)上的ALP表达最高。 TiO 2量的增加降低了复合涂层的生物活性。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号