Long-term experiences with an asphalt membrane at Agger Dam

机译:在Agger大坝上使用沥青膜的长期经验

获取原文
获取原文并翻译 | 示例

摘要

In 1967 the Agger Dam, a 45 m high concrete gravity dam build 1927 to 1929 with 19,300 X 10~3 Mio. m~3 storage, was supplied with a composite sealing made of a 12 cm asphalt membrane and a 28 cm concrete wall. The reinforced concrete covers the asphalt concrete and leads the weight of the new construction to the solid concrete of the old dam by anchorage with 1 meter distance between each other. The leakage rate from the reservoir into the dam drop down to 10 to 20 cm~3/s till today. In 2002 the anchorage plates need a new corrosion protection and the surface of the 1967th concrete has to be rehabilitated. The Aggerverband decided to remove a 1.5 cm concrete layer and supply a 3.0 cm Shot-Polymer-Cement-Concrete (SPCC). After this the Aggerverband expects another lifecycle of at least 30 years of operation for the asphalt membrane.
机译:1967年建造的Agger大坝是一座45 m高的混凝土重力坝,建于1927年至1929年,强度为19,300 X 10〜3Mio。在m〜3的仓库中,提供了由12 cm沥青膜和28 cm混凝土墙制成的复合密封条。钢筋混凝土覆盖沥青混凝土,并通过彼此之间相距1米的锚固将新建筑的重量引至旧水坝的固体混凝土。直到今天,从水库到大坝的泄漏率下降到10至20 cm〜3 / s。在2002年,锚固板需要进行新的腐蚀防护,并且必须修复1967th混凝土的表面。 Aggerverband决定移除1.5厘米的混凝土层,并提供3.0厘米的弹射聚合物水泥混凝土(SPCC)。此后,Aggerverband期望沥青膜的使用寿命至少达到30年。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号