In summary, we try to increase the device performance by adding FA~+ to MA~+. As the concentration of MA_(0.8)FA_(0.2) -PbI_(3-y)Cl_y increases, the PCE will increase, and 1.7 M MA_(0.8)FA_(0.2)PbI_(3-y)Cl_y gives the best photovoltaic performance. To get high performance lead-reduced PSCs, we combine Ba~(2+) substitution of Pb~(2+) with 1.7 M MA_(0.8)FA_(0.2) -PbI_(3-y)Cl_y. When 5.0 mol% Ba~(2+) is doped, the best MA_(0.8)FA_(0.2)Ba_(0.05)Pb_(0.95)I_(3-y)Cl_y device gives V_(oc) of 1.06 V, J_(sc) of 22.3 mA/cm~2, FF of 70.4% and PCE of 16.6%.
机译:总之,我们尝试通过将FA〜+添加到MA〜+来提高设备性能。随着MA_(0.8)FA_(0.2)-PbI_(3-y)Cl_y的浓度增加,PCE将增加,并且1.7 M MA_(0.8)FA_(0.2)PbI_(3-y)Cl_y提供最佳的光伏性能。为了获得高性能的铅还原PSC,我们将Bab(2+)的Ba〜(2+)替代与1.7 M MA_(0.8)FA_(0.2)-PbI_(3-y)Cl_y结合起来。当掺杂5.0 mol%Ba〜(2+)时,最佳MA_(0.8)FA_(0.2)Ba_(0.05)Pb_(0.95)I_(3-y)Cl_y器件给出的V_(oc)为1.06 V,J_( sc)为22.3 mA / cm〜2,FF为70.4%,PCE为16.6%。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号