首页> 外国专利> METHOD FOR PRODUCING LIQUID PIG IRON FROM A DRI PRODUCT

METHOD FOR PRODUCING LIQUID PIG IRON FROM A DRI PRODUCT

机译:从DRI产品生产液体猪铁的方法

摘要

The invention relates to a method for producing liquid pig iron, comprising the following steps: i) providing a directly reduced iron product (1) (DRI product) with an iron content of at least 75.0 wt.%, a carbon content of at least 0.10 wt.% and a content of acids and basic slag components, selected from the group comprising CaO, SiO2, MgO and AI2O3, of max. 15.0 wt.%; ii) supplying the DRI product (1), adding slag formers (2), into an electrically operated smelting unit (3); iii) optionally supplying further iron and/or carbon components (5) into the electrically operated smelting unit (3); iv) smelting the DRI product (1) and optionally the further iron and/or carbon components (5) in the presence of the slag former (2), such that a liquid pig iron phase (6) and a liquid slag phase (7) are formed; v) adjusting the slag phase (7) in such a way that it has a basicity of (CaO+MgO/SiO2) from 0.95 to 1.5; vi) tapping the liquid pig iron phase (6); and vii) tapping and granulating the slag phase (7).
机译:本发明涉及一种制备液体猪铁的方法,包括以下步骤:i)提供直接还原的铁产物(1)(DRI产物),铁含量至少为75.0重量%,至少为碳含量0.10重量%和酸和碱性浆料组分的含量,选自包含CaO,SiO 2,MgO和最大Ai2O3的基团。 15.0重量%; ii)提供DRI产品(1),将炉渣成型器(2)加入电动熔炼单元(3)中; iii)任选地将进一步的铁和/或碳成分(5)供应到电动熔炼单元(3)中; IV)在炉渣前(2)存在下熔化DRI产物(1)和任选的其他铁和/或碳成分(5),使得液体猪铁相(6)和液体渣相(7 ) 形成; v)以这样的方式调节渣相(7),使其具有0.95至1.5的(CaO + MgO / SiO 2)的碱性; vi)挖掘液体猪铁相(6);和vii)敲击和造粒渣相(7)。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号