TITANYL SULFATE HYDRATE POWDER, METHOD FOR PRODUCING TITANYL SULFATE HYDRATE POWDER, METHOD FOR PRODUCING AQUEOUS TITANYL SULFATE SOLUTION, METHOD OF PRODUCING ELECTROLYTE SOLUTION, AND METHOD FOR PRODUCING REDOX FLOW BATTERY

机译:硫酸钛硫酸酯水合物粉末,生产钛硫酸酯水合物粉末的方法,生产含水钛硫酸盐水溶液的方法,生产电解质溶液的方法,以及生产氧化还原流量的方法

摘要

There is provided a titanyl sulfate hydrate powder comprising 25 to 40% by mass of titanium element in terms of TiO2, 40 to 60% by mass of sulfur element in terms of H2SO4, and niobium element in such an amount that a molar ratio of niobium element to titanium element (Nb/Ti) is 0.00005 to 0.012, with a molar ratio of the sulfur element content to the titanium element content (S/Ti) being 1.1 to 1.5, and comprising crystalline titanyl sulfate dihydrate (TiOSO4.2H2O). Thus, the present invention can provide a titanyl sulfate hydrate powder with a high dissolution rate in water and a production method therefor, as well as a method for producing an aqueous titanyl sulfate solution, a method for producing an electrolyte and a method for producing a redox flow battery, using the titanyl sulfate hydrate powder.
机译:提供了在H 2 SO 4的TiO 2,40至60质量%的硫磺元素方面提供了包含25至40质量%的硫酸钛元素的钛硫酸盐水合物粉末,并以铌的摩尔比的量 钛元素(Nb / Ti)的元素为0.00005至0.012,具有硫元素含量与钛元素含量(S / Ti)的摩尔比为1.1至1.5,并包含结晶硫酸钛硫酸盐二水合物(Tioso4.2H2O)。 因此,本发明可以在水中提供具有高溶解速率的硫酸钛水合物粉末及其制备方法,以及制备硫酸盐水溶液水溶液的方法,一种用于生产电解质的方法和制造方法的方法 氧化还原流动电池,使用硫酸钛水合物粉末。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号