首页> 外国专利> TITANYL SULFATE HYDRATE POWDER, METHOD FOR PRODUCING TITANYL SULFATE HYDRATE POWDER, METHOD FOR PRODUCING AQUEOUS TITANYL SULFATE SOLUTION, METHOD OF PRODUCING ELECTROLYTE SOLUTION, AND METHOD FOR PRODUCING REDOX FLOW BATTERY

TITANYL SULFATE HYDRATE POWDER, METHOD FOR PRODUCING TITANYL SULFATE HYDRATE POWDER, METHOD FOR PRODUCING AQUEOUS TITANYL SULFATE SOLUTION, METHOD OF PRODUCING ELECTROLYTE SOLUTION, AND METHOD FOR PRODUCING REDOX FLOW BATTERY

机译:硫酸钛硫酸酯水合物粉末,制备硫酸钛水合物粉末的制备方法,制备硫酸盐水溶液水溶液的方法,生产电解质溶液的方法,以及生产氧化还原流电池的方法

摘要

There is provided a titanyl sulfate hydrate powder comprising 25 to 40% by mass of titanium element in terms of TiO2, 40 to 60% by mass of sulfur element in terms of H2SO4, and niobium element in such an amount that a molar ratio of niobium element to titanium element (Nb/Ti) is 0.00005 to 0.012, with a molar ratio of the sulfur element content to the titanium element content (S/Ti) being 1.1 to 1.5, and comprising crystalline titanyl sulfate dihydrate (TiOSO4·2H2O). Thus, the present invention can provide a titanyl sulfate hydrate powder with a high dissolution rate in water and a production method therefor, as well as a method for producing an aqueous titanyl sulfate solution, a method for producing an electrolyte and a method for producing a redox flow battery, using the titanyl sulfate hydrate powder.
机译:提供了硫酸钛硫酸盐水合物粉末,其在TIO 2 ,40至60质量%的硫元素方面,在H 2时,硫酸淀粉元素为25至40质量%。亚磷酸盐脱碘元素,铌元素与钛元素(Nb / Ti)的摩尔比为0.00005至0.012,硫比与硫元素含量与摩尔比为0.00005至0.012钛元素含量(S / TI)为1.1至1.5,并包含结晶硫酸酯二水合物(Tioso 4 ·2H 2 O)。因此,本发明可以在水中提供具有高溶解速率的硫酸钛水合物粉末及其制备方法,以及制备水性硫酸酯水溶液的方法,一种用于产生电解质的方法和制造方法的方法氧化还原流量电池,使用硫酸钛水合物粉末。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com