Method for producing short fiber anionic cellulose modified fiber

机译:生产短纤维阴离子纤维素改性纤维的方法

摘要

An anionic modified cellulose fiber containing a step of dissolving a sugar chain by thermal decomposition under a temperature condition of 50 to μ Over 500 μ The method of producing a short fibrous anionic modified cellulose fiber that is less than m is an average fiber length of anionic modified cellulose fiber μ More than μ Manufacturing method which is m or less.By using a short fiber anionic modified cellulose fiber obtained by the manufacturing method of the present invention, it is possible to prepare a dispersion containing a highly concentrated cellulose fiber having a high concentration and low viscosity and high handling ability, and packaging materials for daily use goods, household electric appliances, and household appliances It can be suitably used for various industrial applications such as automobile parts and three-dimensional molding materials.
机译:阴离子改性纤维素纤维纤维,其在50至μ的温度条件下通过热分解溶解糖链的步骤超过500μm,其产生短于m的短纤维阴离子改性纤维素纤维的方法是阴离子的平均纤维长度改性纤维素纤维μ多于μ制造方法,其为m或更小。通过通过本发明的制造方法获得的短纤维阴离子改性纤维素纤维,可以制备含有高浓度纤维素纤维的分散体浓度和低粘度和高处理能力,以及日常使用的包装材料,家用电器和家用电器可适合用于各种工业应用,如汽车零件和三维成型材料。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号