PROBLEM TO BE SOLVED: To provide a method for producing a silk fiber three-dimensional structure in a biologically safe process, using silk protein of high biocompatibility, which can be used in the fields of regenerative medicines and perfume cosmetics and the like.SOLUTION: A silk fiber three-dimensional structure is produced by using silk protein aqueous solution with a concentration of 4w/v% or more and 22 w/v% or less and a pH of 8-12 as spinning solution, according to electric field spinning.SELECTED DRAWING: Figure 1
机译:要解决的问题:提供一种在生物安全方法中生产丝纤维三维结构的方法,使用高生物相容性的丝蛋白,可用于再生药物和香水化妆品等。案例:根据电场纺丝,通过使用浓度为4w / v%或更高,22 w / v%或更低的浓度为4w / v%或更高,22 w / v%或更低,pH为8-12的pH来产生丝纤维三维结构。选定的绘图:图1

著录项

  • 公开/公告号JP6842687B2

    专利类型

  • 公开/公告日2021-03-17

    原文格式PDF

  • 申请/专利权人 国立大学法人信州大学;

    申请/专利号JP20160173094

  • 申请日2016-09-05

  • 分类号D01F4/02;A61L27/22;A61L15/32;A61K8/64;A61K35/64;A61Q19;A61P17/16;A61P17/02;B01D39/16;

  • 国家 JP

  • 入库时间 2022-08-24 17:44:30

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号