The present invention discloses a method for preparing a vanadium battery electrolyte by using a waste vanadium catalyst. The method includes step A: soaking a waste vanadium catalyst in an oxalic acid solution for 2-8 h, to generate a solution containing vanadyl oxalate; step B: cleaning the waste vanadium catalyst, and collecting the vanadyl oxalate solution; and step C: adding a polyacid ester into the vanadyl oxalate solution; and after full reaction, removing impurities by filtration, and concentrating the filtrate to obtain a vanadyl oxalate mother solution. The method for preparing a vanadium battery electrolyte by using a waste vanadium catalyst according to the present invention does not generate wastes which cause environmental pollution in the treatment process, and can make a solution in the waste vanadium catalyst treatment process generate the electrolyte for preparing a vanadium battery. The process is simple and the treatment cost is low.
机译:本发明公开了一种通过使用废钒催化剂制备钒电池电解质的方法。该方法包括步骤a:将废钒催化剂浸泡在草酸溶液中2-8小时,以产生含有草酸钒酸甲酯的溶液;步骤B:清洁废钒催化剂,并收集草酸钒酸盐溶液;步骤C:将多酸酯添加到草酸甲酸盐溶液中;在完全反应后,过滤除去杂质,并浓缩滤液以获得草酸钒母溶液。使用根据本发明的废钒催化剂制备钒电池电解质的方法不会产生导致治疗过程中环境污染的废物,并且可以使废钒催化剂处理过程中的溶液产生用于制备的电解质钒电池。该过程简单,治疗成本低。

著录项

  • 公开/公告号US2021061672A1

    专利类型

  • 公开/公告日2021-03-04

    原文格式PDF

  • 申请/专利权人 HUNAN SANFENG VANADIUM INDUSTRY CO. LTD.;

    申请/专利号US201916558901

  • 发明设计人 XIAODI XU;XINGJIANG TIAN;

    申请日2019-09-03

  • 分类号C01G31;H01M10/0562;

  • 国家 US

  • 入库时间 2022-08-24 17:30:27

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号