首页> 外国专利> Method of and apparatus for solder coating a lead and a method of soldering a lead coated by the method

Method of and apparatus for solder coating a lead and a method of soldering a lead coated by the method

机译:用于焊料涂覆引线的方法和设备以及通过该方法焊接涂覆的引线的方法

摘要

776,378. Coating with metals. ERIE RESISTOR CORPORATION". Nov. 26. 1954 [Jan. 25, 1954], No. 34359/54. Class 82(2) [Also in Groups XXII and XXXVI] A copper lead is coated with soft solder by passing the lead through a bath of soft solder and then through a column of heated oil floating on the surface of the solder, the oil being at such a temperature as ,to set the solder to the lead. A tinned copper wire 9, Fig. 6, is passed through a flux bath 10 under pulleys 11, through a molten solder bath 13 at 440-470‹F. under pulleys 14, 15 and then up through a cylinder 16 filled with palm oil floating on the solder, the average temperature of the oil being' 100- 200‹F. below the solder bath temperature to smooth and set the solder coating. The oil is circulated by a pump 22 and cooled in a heat exchanger 20. The coated wire is cleaned in a solvent bath 24. Two such coated wires are soldered to the ends of a condenser.
机译:776,378。用金属涂层。 ERIE RESISTOR CORPORATION”。1954年11月26日[1954年1月25日],编号34359/54。Class 82(2)[也属于XXII和XXXVI组]通过使软导线穿过在软焊料浴中,然后通过一列漂浮在焊料表面的加热油,使油处于的温度下,以将焊料固定在铅上,并通过镀锡铜线9(图6)。通过皮带轮11下的助熔剂槽10,通过皮带轮14、15下440-470°F的熔融焊料槽13,然后经过装有浮在焊料上的棕榈油的圆柱体16向上,油的平均温度为在低于锡浴温度100-200°F的温度下使焊料涂层光滑并凝固,油通过泵22循环并在热交换器20中冷却。在溶剂浴24中清洗涂覆的导线。电线被焊接到电容器的末端。

著录项

  • 公开/公告号GB776378A

    专利类型

  • 公开/公告日1957-06-05

    原文格式PDF

  • 申请/专利权人 ERIE RESISTOR CORPORATION;

    申请/专利号GB19540034359

  • 发明设计人

    申请日1954-11-26

  • 分类号H01G13/00;

  • 国家 GB

  • 入库时间 2022-08-23 22:11:08