Injection mouldable rapid-cure, epoxy! resin compsns. - contg. hexa:hydro-phthalic anhydride and 2,4,6-tri(dimethylaminomethyl)-phenol, esp. for pressure gelation injection moulding

机译:注塑可快速固化,环氧树脂!树脂组合物。 -续六:氢邻苯二甲酸酐和2,4,6-三(二甲基氨基甲基)苯酚,特别是用于压力凝胶注射成型

摘要

Compsns. are based on (a) a liq. unmodified epoxy resin; (b) methyl hexahydrophthalic anhydride (I) as cross linking agent; (c) 2,4,6-tri-(dimethylaminomethyl)-phenol as accelerator (II) and (d) opt. fillers and pigments. The compsns. are esp. useful for the injection moulding of electrical insulation components. They contain no components which detract from the excellent mechanical, electrical and chemical resistant properties of the epoxy resin. The compsns. cure 4-5 times more rapidly than prior art epoxy resins. A 5-10 kg pressure injected bisphenol-A epoxy resin-based moulding gels in 2-3 mins. at 3-5 atmos. pressure and 165 degrees C.
机译:Compsns。基于(a)液体未改性的环氧树脂; (b)甲基六氢邻苯二甲酸酐(I)作为交联剂; (c)2,4,6-三-(二甲基氨基甲基)-苯酚作为促进剂(II),(d)选择。填料和颜料。 compsns。特别是用于电气绝缘组件的注塑成型。它们不包含不利于环氧树脂优异的机械,电气和化学耐性的组分。 compsns。固化速度是现有技术环氧树脂的4-5倍。在2-3分钟内以5-10 kg压力注入双酚A环氧树脂基成型胶。在3-5个大气压下。压力和165摄氏度。

著录项

  • 公开/公告号FR2379558B3

    专利类型

  • 公开/公告日1980-10-10

    原文格式PDF

  • 申请/专利权人 MUANYAGIPARI KUTATO INTEZET;

    申请/专利号FR19780002870

  • 发明设计人

    申请日1978-02-02

  • 分类号C08G59/42;C08G59/68;C08L63/02;

  • 国家 FR

  • 入库时间 2022-08-22 17:24:12