improved lining material attached to the training of the materials and methods.

机译:改进了衬里材料,对材料和方法进行了培训。

摘要

hardened composition obtained from the joint of a mixture consisting of,weight: 100 parts of a binder based on rubber and from about 5 to about 1000 parts of rice husks powder, and from about 1 to about 200 parts of a polyester derived from the mmonomer with a diol or diacid and at least one acid derivative monomer.the said polyester is at least partially crystalline at ambient conditions and having a glass transition temperature of approximately 50 degrees to 80 degrees c and approximately molecular weightan average weight of about 1000 to about 500000.the rice husks as backup and load in combination with the rubber and polyester, are able to comply with the joint defects of flanges.
机译:由以下混合物的混合物得到的硬化组合物:重量:100份橡胶基粘合剂和约5份至1000份稻壳粉,以及约1份至200份源自单体的聚酯具有二醇或二酸和至少一种酸衍生物单体。所述聚酯在环境条件下至少部分结晶,并且具有约50至80℃的玻璃化转变温度和约1000至约500000的分子量。 。稻壳作为支撑和负载,与橡胶和聚酯结合使用,能够应对法兰的接缝缺陷。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号