Ladle for receiving and optionally after-treating and/or transporting hot liquid metals.

机译:钢包,用于接收和可选地进行后处理和/或运输热液态金属。

摘要

Ladle for receiving and, where necessary, for subsequent treatment and/or transportation of hot, molten, metals which are poured from a preceding melting unit into the ladle (10), which a lining (14) made of high-temperature-resistant material such as, for example, chamotte bricks which lie adjacent to one another and cover the base and side walls of the ladle and have, at the point of impact (18) of the pouring stream of molten metal (19), an impact element which projects above the adjacent surface (23) of the lining (14), characterized in that the impact element is a domed element (20) inset into the lining (14), of which the domed surface (22) is directed against the pouring stream of molten metal and blends without a step into the surface (23) of the adjacent lining (17) and of which the smallest diameter D or the smallest edge length at the transition to this surface (23) is larger than the diameter (d) of the pouring stream of molten metal (19) at the point of impact (18).
机译:钢包,用于接收和在必要时进行后续处理和/或运输,从先前的熔化装置浇注到钢包(10)中的热的熔融金属,钢包(10)由耐高温材料制成诸如例如紧挨着并覆盖钢包底壁和侧壁的粘土砖,并且在熔融金属(19)的浇注流(18)的冲击点(18)上具有一个冲击元件,突出部在衬里(14)的相邻表面(23)上方突出,其特征在于,冲击元件是嵌入衬里(14)中的圆顶形元件(20),其中圆顶形表面(22)指向浇注流熔融金属和混合气,没有台阶进入相邻衬里(17)的表面(23),并且在过渡到该表面(23)时的最小直径D或最小边缘长度大于直径(d)冲击点(18)处熔融金属(19)的浇注流量的变化。

著录项

  • 公开/公告号ES296282U

    专利类型

  • 公开/公告日1987-09-01

    原文格式PDF

  • 申请/专利权人 FIRMA LICHTENBERG FEUERFEST GMBH.;

    申请/专利号ES19850296282U

  • 发明设计人

    申请日1985-10-29

  • 分类号B22D41/02;

  • 国家 ES

  • 入库时间 2022-08-22 07:17:30