A method of obtaining a recrystallised alloy based on aluminum

机译:一种获得基于铝的再结晶合金的方法

摘要

Products made of Al alloy containing from 1 to 3.5% of Li, up to 4% of Cu, up to 5% of Mg, up to 3% of Zr and additions of Mn, Cr and/or Zr in the following quantities by weight:… Zr /= 0.10% - Mn /= 0.8% - Cr /= 0.20%… with %Zr/0.03 + %Mn/0.3 + %Cr/0.07 1. …??The alloy is recrystallised and has a grain size smaller than 200  mu m. …??The manufacturing range essentially comprises a final subtempering at temperatures lower than or equal to the temperature resulting in the maximum hardening of the alloy and for periods shorter than those resulting in maximum hardening at each temperature.
机译:由铝合金制成的产品,其中含有1-3.5%的Li,最多4%的Cu,最多5%的Mg,最多3%的Zr和以下重量比的Mn,Cr和/或Zr添加量:…Zr 1。…合金重结晶晶粒尺寸小于200微米。 …制造范围基本上包括在低于或等于导致合金最大硬化的温度下的最终子回火,并且持续时间短于导致在每个温度下最大硬化的那些时间。

著录项

  • 公开/公告号ES556496A0

    专利类型

  • 公开/公告日1987-12-16

    原文格式PDF

  • 申请/专利号ES19860556496

  • 发明设计人

    申请日1986-06-24

  • 分类号C22C21/08;C22F1/047;

  • 国家 ES

  • 入库时间 2022-08-22 06:57:21

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号