PCT No. PCT/SU87/00023 Sec. 371 Date Oct. 5, 1988 Sec. 102(e) Date Oct. 5, 1988 PCT Filed Feb. 16, 1987 PCT Pub. No. WO88/06190 PCT Pub. Date Aug. 25, 1988.The hereinproposed method and furnace provide for preliminary building up of melt in a melting pot (10) of a rectangular shape in the horizontal section, delivery of an oxygen-containing gas (3) into the melt below its surface level through tuyeres (13) with nozzles (14) installed in the longer walls of the melting pot (10) creating two melt zones: an upper zone (9) loaded with solid carbon fuel (2) in an amount sufficient for providing a volumetric concentration of said fuel within 0.5 to 50% of the melt volume in said zone (9), wherein said concentration is maintained by subsequent concurrent loading of iron-bearing material (1) and solid carbon fuel (2), and a lower zone (8) consisting of a layer of slag (4) and a layer of ferrocarbon intermediate product (5) said layers being discharged separately through channels (17 and 18) made in the counterproposed short walls of the melting pot (10). The ratio of the horizontal section area of the melting pot (10) at the installation level therein of tuyeres (13) to the total area of the outlet holes of the nozzles (14) is 300-10000, while the distance (h) from the lower boundary of the product discharge channel (18) to the upper boundary of the slag discharge channel (17) is 0.3 to 0.75 the distance (H) from the lower boundary of the product discharge channel (18) to the installation level of the tuyeres (13).
机译:PCT号PCT / SU87 / 00023秒371日期1988年10月5日第102(e),1988年10月5日,PCT,1987年2月16日,PCT公开。 WO88 / 06190 PCT公开号1988年8月25日,本文提出的方法和熔炉提供了在水平截面为矩形的熔炉(10)中初步建立熔体的构造,将含氧气体(3)输送到熔体下方的熔体中。通过安装在熔炉(10)较长壁上的喷嘴(14)穿过风口(13)形成两个水平的熔体区域:上部区域(9)装有足以提供燃料的固体碳燃料(2)在所述区域(9)中所述燃料的体积浓度在熔体体积的0.5%至50%之内,其中通过随后同时加载含铁材料(1)和固体碳燃料(2)以及下部区域来保持所述浓度(8)由炉渣层(4)和铁碳中间产物层(5)组成,所述各层分别通过在熔炉(10)的相对短壁中制成的通道(17和18)排出。风口(13)在其安装高度处的熔炉(10)的水平截面积与喷嘴(14)的出口孔的总面积之比为300-10000,而距熔炉(10)的距离(h)为产物排出通道(18)的下边界到矿渣排出通道(17)的上边界的距离为从产物排出通道(18)的下边界到炉渣安装高度的距离(H)为0.3至0.75。风口(13)。

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号