PURPOSE:To provide the subject crushing agent attached to a reinforcing steel cage before the application of concrete to facilitate an excessive concrete- removing work by mixing calcined lime, etc., with at least one of a saccharide, an alkali silicofluoride and a specific hydraulic setting material. CONSTITUTION:Calcined lime and/or calcined dolomite are mixed with a combi nation of at least one kind selected from (A) 0.05-5 wt.% (preferably 0.1-2 wt.%)of a saccharide, a polyhydric alcohol and an organic acid (salt), (B) 0.05-10 wt.% (preferably).1-5 wt.%) of an alkali silicofluoride and (C) 1-50 wt.% (prefer ably 5-30 wt.%) of a hydraulic setting material comprising (i) a hydraulic setting material containing 11CaO.7Al2O3.CaF2, (ii) hydraulic setting material containing 12CaO.7Al2O3 and (iii) a hydraulic setting material containing 3CaO.3 Al2O3.CaSO4 to provide the objective crushing agent.
机译:用途:在将混凝土煅烧后,将煅烧的石灰等与糖,碱式氟化硅和特定的水硬性酸中的至少一种混合,以提供一种附着在钢筋笼上的粉碎剂,以促进过度的混凝土去除工作。设置材料。组成:煅烧石灰和/或煅烧白云石与至少一种选自以下的组合:糖类,多元醇和有机物的0.05-5 wt。%(优选0.1-2 wt。%)酸(盐),(B)氟化硅碱0.05-10 wt。%(优选).1-5 wt。%和(C)1-50 wt。%(优选5-30 wt。%)包括(i)包含11CaO.7Al2O3.CaF2的水硬性材料,(ii)包含12CaO.7Al2O3的水硬性材料和(iii)包含3CaO.3 Al2O3.CaSO4的水硬性材料以提供目标破碎剂的水硬性材料。

著录项

  • 公开/公告号JPH03243681A

    专利类型

  • 公开/公告日1991-10-30

    原文格式PDF

  • 申请/专利权人 SUMITOMO CEMENT CO LTD;

    申请/专利号JP19900038359

  • 发明设计人 SATO MASAO;YAMADA SOTA;KAWASAKI HISAMI;

    申请日1990-02-21

  • 分类号E02D5/34;B02C19/18;C09K3/00;

  • 国家 JP

  • 入库时间 2022-08-22 06:04:00

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号