PURPOSE: To provide the centrifugal casting method capable of obtaining a ductile cast iron tube having high strength/elongation and excellent toughness even though a tube thickness is thin. ;CONSTITUTION: A ductile cast iron molten metal is produced by adding graphite spherodizer in the source molten metal melted by melting furnace, subjecting to inoculation on the molten metal and casting into the mold for centrifugal casting, a ductile cast iron tube is centrifugally cast. At this time, the treatment for spherodizing graphite is executed with using Mg alloy containing a rare metal element, a ductile cast iron molten metal, which contains, by weight, 2.1-2.5% Si, 0.04-0.06% Mg in the case of using the source molten metal melted by cupola (or 2.6-2.8% Si, 0.03-0.06% Mg in the case of using the source molten metal melted by electric furnace), is produced, the molten metal is subjected to inoculation to the molten metal and is cast into the mold for centrifugal casting having a powder layer of inoculant on its inside surface.;COPYRIGHT: (C)1994,JPO&Japio
机译:目的:提供一种离心铸造方法,即使管厚度薄,也能够获得具有高强度/伸长率和优异韧性的球墨铸铁管。组成:球墨铸铁熔融金属是通过在熔化炉熔化的原料熔融金属中加入石墨球化剂,然后在熔融金属上接种然后浇铸到离心铸造模具中而制成的,球墨铸铁管进行离心铸造。此时,通过使用包含稀有金属元素的Mg合金,球墨铸铁熔融金属来进行石墨化处理,球墨铸铁熔融金属以重量计包含2.1-2.5%的Si,在使用的情况下为0.04-0.06%的Mg。产生通过冲天炉熔融的原料熔融金属(或者在使用电炉熔融的原料熔融金属的情况下为2.6-2.8%Si,0.03-0.06Mg),对熔融金属进行接种。浇铸到离心铸造的模具中,该模具的内表面具有孕育剂粉末层。;版权所有:(C)1994,JPO&Japio

著录项

  • 公开/公告号JPH06246415A

    专利类型

  • 公开/公告日1994-09-06

    原文格式PDF

  • 申请/专利权人 KUBOTA CORP;

    申请/专利号JP19930037017

  • 发明设计人 TAKEUCHI KATSUYUKI;KUROTOBI MANABU;

    申请日1993-02-25

  • 分类号B22D13/02;B22D1/00;B22D13/10;C22C33/10;C22C37/04;

  • 国家 JP

  • 入库时间 2022-08-22 04:49:21

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号