METHOD FOR CASTING NB-CONTAINING FERRITIC STAINLESS STEEL BY TWIN ROLL CONTINUOUS CASTING METHOD

机译:双辊连续铸造法铸造含NB的铁素体不锈钢的方法

摘要

PURPOSE: To provide a casting method, by which surface crack on a cast strip can be reduced to a practically allowable extent, related to the method for casting an Nb-containing ferritic stainless steel by a twin roll continuous casting method. ;CONSTITUTION: In the method for casting the ferritic stainless steel containing 0.001-0.03wt.% C, 0.2-1.0% Si, 0.05-0.8% Mn, ≤0.03% P, ≤0.01% S, 0.1-5.0% Nb and 0.001-0.03% N into the cast strip having 1-6mm thickness by the twin roll type continuous casting method, the cooling speed of the cast strip is set at ≥10000°C/min from the time when the cast strip comes out from the cooling rolls to the time when the temp. lowers to 1200°C and at ≥1500°C/min from 1200°C to 800°C and thereafter, water cooling is executed to prevent the precipitation and the growth of NbCN at high temp.;COPYRIGHT: (C)1994,JPO&Japio
机译:目的:提供一种通过双辊连续铸造法铸造含Nb铁素体不锈钢的方法,通过该铸造方法可将铸造带材上的表面裂纹减少到实际允许的程度。 ;组成:在铸造含0.001-0.03wt。%C,0.2-1.0%Si,0.05-0.8%Mn,≤0.03%P,≤0.01%S,0.1-5.0%Nb和0.001的铁素体不锈钢的方法中通过双辊式连续铸造法向厚度为1-6mm的铸带中添加-0.03%N,从铸带从冷却出来时算起,铸带的冷却速度设置为≥10000°C / min滚动到温度从1200°C降至800°C并以≥1500°C / min的速度降到1200°C,然后进行水冷却以防止NbCN在高温下析出和生长.COPYRIGHT:(C)1994,JPO&Japio

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号