Method for improving the heap biooxidation rate of refractory sulfide ore particles that are biooxidated using recycled bioleachate solution
Method for improving the heap biooxidation rate of refractory sulfide ore particles that are biooxidated using recycled bioleachate solution
展开▼
机译:利用回收的生物浸出液提高生物氧化度的难熔硫化物矿石颗粒堆生物氧化率的方法
展开▼
页面导航
摘要
著录项
相似文献
摘要
A method for improving the heap biooxidation rate of refractory sulfide ore particles that are at least partially biooxidized using a recycled bioleachate off solution is provided. The method includes the steps of biooxidizing a heap of refractory sulfide ore particles with a bioleachate solution; collecting, from the heap, a bioleachate off solution that includes a plurality of inhibitory materials dissolved therein, the concentration of each individual inhibitory material being below its individual inhibitory concentration but the combined concentration of at least two of the inhibitory materials being sufficient to inhibit the biooxidation rate of the refractory sulfide ore particles; conditioning the bioleachate off solution to reduce the inhibitory effect caused by the combined concentration of the at least two inhibitory materials; recycling the reconditioned bioleachate solution to the to the heap; and biooxidizing the refractory sulfide ore particles in the heap with the reconditioned bioleachate solution.
展开▼