The present invention relates to a method for processing a peacock pattern stone for mining the peacock pattern in a mountain area so that it can be widely used in various building materials or ornamental, jewelry, etc. (Iii) After heating for 7 to 8 hours with air pressure of 0.3K / m² at 1210 ℃ ~ 1250 ℃ and cooling for 3 hours in furnace, it is 1215 ℃ ~ 1220 in furnace without exhaust pipe. ℃, air pressure 0.2K / m², gas pressure 1.3K / m² or 1215 ℃ and 0.5K / m², gas pressure 0.5K / m², gas pressure 0.5K / m² It is.;As mentioned above, by processing the non-patterned peacock pattern at high temperature and changing it into bluish green, dark gray, black, etc., it makes the pattern clear and makes cutting easy. It is a very beneficial invention that can be used extensively as glazing of tiles.
机译:孔雀纹石的加工方法技术领域本发明涉及一种用于在山区开采孔雀纹的孔雀纹石的加工方法,使其可广泛用于各种建材或装饰物,珠宝等。(ii)加热7至8小时后在1210℃〜1250℃的空气压力为0.3K /m²的情况下,在炉内冷却3小时,在不带排气管的炉内为1215℃〜1220。 ℃,气压为0.2K /m²,气压为1.3K /m²或1215℃和0.5K /m²,气压为0.5K /m²,气压为0.5K /m²。如上所述,通过加工非在高温下将孔雀图案制成图案,然后将其更改为蓝绿色,深灰色,黑色等,使图案清晰且易于切割。这是非常有益的发明,可以广泛用作瓷砖的上光。

著录项

  • 公开/公告号KR970058866A

    专利类型

  • 公开/公告日1997-08-12

    原文格式PDF

  • 申请/专利权人 정재일;

    申请/专利号KR19970020888

  • 发明设计人 정재일;

    申请日1997-05-24

  • 分类号B28D1/00;

  • 国家 KR

  • 入库时间 2022-08-22 03:16:26

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号