1. A method for producing fine-grained corundum, aluminum comprising treating the oxygenate compounds at 350 - 450 o C and pressure of water vapor in the presence of an activator ion type, characterized in that the oxygen-containing compounds is a hydroxide or oxide of aluminum, and the activator compound are used the ionic type containing anions selected from the group of nitrates, sulfates, chromates, borates, acetates and hydroxyl ions and water vapor pressure is maintained at 30 - 400 atm.; 2. The method of claim. 1, characterized in that used as an activator potassium hydroxides, sodium, barium, aluminum or alkylammonium.; 3. The method of claim. 1, characterized in that the activator used is sodium chromate or cadmium tetraborate.; 4. The method of claim. 1, characterized in that the activator is used lanthanum nitrate, potassium dichromate or potassium alum.; 5. The method of claim. 1, characterized in that the activator used as barium nitrate, magnesium acetate, copper sulphate or nickel sulphate.; 6. The method of claim. 1, characterized in that the activator is used chromium nitrate, ammonium dichromate, or boric acid.
机译:1.一种生产细粒刚玉铝的方法,该方法包括在活化剂离子类型的存在下,在350-450℃和水蒸气压力下处理含氧化合物,其特征在于,氧-含有化合物的是铝的氢氧化物或氧化物,并且活化剂化合物使用的离子型含有选自硝酸根,硫酸根,铬酸根,硼酸根,乙酸根和氢氧根离子的阴离子,并且水蒸气压力保持在30-400atm。 ; 2.权利要求的方法。 1,特征在于用作活化剂的氢氧化钾,钠,钡,铝或烷基铵。 3.权利要求的方法。 1,特征在于所用的活化剂是铬酸钠或四硼酸镉。 4.权利要求的方法。 1,特征在于该活化剂是使用硝酸镧,重铬酸钾或明矾钾。 5.权利要求的方法。 1,特征在于该活化剂用作硝酸钡,乙酸镁,硫酸铜或硫酸镍。 6.权利要求的方法。 1,特征在于活化剂是使用硝酸铬,重铬酸铵或硼酸。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号