首页> 外国专利> PAVEMENT METHOD USING WATER-PERMEABLE RESIN PAVEMENT MATERIAL, AND MANUFACTURE OF BLOCK

PAVEMENT METHOD USING WATER-PERMEABLE RESIN PAVEMENT MATERIAL, AND MANUFACTURE OF BLOCK

机译:使用透水性树脂铺面材料的铺面方法及块的制造

摘要

PROBLEM TO BE SOLVED: To express the color of a material as it is by adding urethane resin to a color glass which is pulverized and whose grain size is regulated to the specific value as aggregate, and mixing the color glass and the urethane resin to form a pavement material in which the urethane resin weight ratio is the specific value. ;SOLUTION: A pavement material to be manufactured by mixing color glass as aggregate whose grain size is regulated to 0-5 mm and urethane resin as a binder with the weight ratio of 5-10 urethane resin to 100 aggregate to be used, is placed on a surface to be executed. The aggregate to be used is regulated in grain size, and water-permeable, and there is not discoloration because no pigment is used in the aggregate, and the color of the material can be expressed as it is. When the urethane resin of the quantity exceeding the limit is used, bubbles are generated, its appearance becomes worse, and the strength is degraded. Because no discoloration is generated in the urethane resin, the color of the material can be expressed as it is.;COPYRIGHT: (C)1999,JPO
机译:解决的问题:通过将尿烷树脂添加到粉碎的有色玻璃中并将其粒度调节到特定值作为聚集体,然后将有色玻璃和尿烷树脂混合以形成材料,以表现材料的颜色聚氨酯树脂的重量比为特定值的路面材料。 ;解决方案:放置一种路面材料,该路面材料是通过混合使用彩色玻璃作为骨料,将其粒度限制为0-5 mm,并使用聚氨酯树脂作为粘合剂,以100的骨料的重量比为5-10的氨基甲酸酯树脂制成的在要执行的表面上。所使用的骨料的粒径和透水性受到调节,并且由于没有在骨料中使用颜料,因此不会变色,并且材料的颜色可以原样表达。当使用数量超过极限的聚氨酯树脂时,会产生气泡,其外观变差,并且强度降低。因为在氨基甲酸酯树脂中不会发生变色,所以可以按原样表示材料的颜色。版权所有:(C)1999,JPO

著录项

  • 公开/公告号JPH11181707A

    专利类型

  • 公开/公告日1999-07-06

    原文格式PDF

  • 申请/专利权人 KONO YUJI;

    申请/专利号JP19970370069

  • 发明设计人 KONO YUJI;

    申请日1997-12-20

  • 分类号E01C7/30;E01C5/22;

  • 国家 JP

  • 入库时间 2022-08-22 02:34:14

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号