首页> 外国专利> Method for reducing the formation of beta phase in the form of primary platelet AlSi alloy containing iron, in particular in alloys of Al - Si - Mn - Fe

Method for reducing the formation of beta phase in the form of primary platelet AlSi alloy containing iron, in particular in alloys of Al - Si - Mn - Fe

机译:减少含铁的初生血小板AlSi合金形式的β相形成的方法,特别是在Al-Si-Mn-Fe合金中

摘要

Method for reducing the formation of beta phase in the form of primary platelet AlSi alloy containing iron, in particular in alloys of Al - Si - Mn - Fe.Iron is a harmful impurity in aluminum alloys, as he does with that the phases intermetu00e1licas rich in iron, hard and brittle palms during solidification.The most damaging in the microstructure is the beta phase of type Al ~ 5 ~ FeSi, due to their form of tag.The present invention provides a production method of alloy of Al containing iron by controlling and regulating the path of precipitation during solidification in such a way that precipitThe action of intermetu00e1licas phases containing Fe starts with the precipitation of hexagonal phase of Al Fe ~ 2 ~ 8 ~ ~ you. The presence of phase type Al ~ 8 ~ Fe ~ 2 ~ you.The presence of phase type Al ~ 8 ~ Fe ~ 2 ~ itself results in the fact that the beta phase will not develop the morphology of platelet common, but will the nuclear phase of type Al ~ 8 ~ Fe ~ 2 ~ you and cover it.That in turn has a morphology less harmful. In addition, the invention defines the use of thermal analysis as a means to control the morphology of the precipitates.
机译:减少含铁的初级片状AlSi合金(特别是在Al-Si-Mn-Fe合金中)的β相形成的方法。铁是铝合金中的有害杂质,因为铁与铝之间的相互变凝固过程中富含铁,硬而脆的手掌。由于其标签形式,在显微组织中最具破坏性的是Al〜5〜FeSi型的β相。本发明提供了一种含铁的Al合金的生产方法通过控制和调节凝固过程中的析出路径,使析出的含铁中间相开始于Al Fe〜2〜8〜〜六角相的析出。相型Al〜8〜Fe〜2〜you的存在。相型Al〜8〜Fe〜2〜本身的存在导致β相不会发展出普通血小板的形态,但会核化Al〜8〜Fe〜2〜相的相并覆盖它,反过来形态学危害较小。另外,本发明定义了使用热分析作为控制沉淀物形态的手段。

著录项

  • 公开/公告号BR9610978A

    专利类型

  • 公开/公告日1999-12-28

    原文格式PDF

  • 申请/专利权人 OPTICAST AB;

    申请/专利号BR19969610978

  • 发明设计人 LENNART BACKERUD;GUOCAI CHAI;LARS ARNBERG;

    申请日1996-10-09

  • 分类号C22C1/02;C22F1/043;

  • 国家 BR

  • 入库时间 2022-08-22 01:57:20