Production method null of metal connotation carbon

机译:金属内涵碳的生产方法无效

摘要

PURPOSE: To enhance the productivity of a metal-contg. carbon cluster, to facilitate collection and to increase the kinds of metallic compds. by pulverizing a metallic element-contg. oxide and a powdery carrier in an org. solvent and carrying out drying, heating in an atmosphere of a hydrogen-contg. reducing gas and heating in a vacuum. CONSTITUTION: A metal oxide and a powdery carrier, preferably alumina, zirconia or manganese oxide are pulverized in an org. solvent to stick the metal oxide of about several μm to the surface of the carrier. The metal oxide is reduced by heating in an atmosphere of a hydrogen-contg. reducing gas and the objective metal-contg. carbon cluster is formed from carbon atoms fed from the adsorbed residual org. solvent or graphite by heating in a vacuum. For example, alumina powder having 20-400 nm diameter is mixed with tungsten oxide powder having several μm diameter and alcohol. After pulverization, the resultant tungsten doped alumina powder 4 with occluded alcohol is put in a graphite vessel 1, the vessel 1 is set in a carbon fiber vessel 3 and the powder 4 is heated with a carbon heater 2 while blowing hydrogen-contg. gaseous Ar.
机译:目的:提高金属加工的生产率。碳簇,以促进收集并增加金属化合物的种类。通过将金属元素粉磨碎。氧化物和组织中的粉状载体。溶剂,干燥,在含氢气氛中加热。减少气体并在真空中加热。组成:金属氧化物和粉末状载体,优选氧化铝,氧化锆或氧化锰在有机炉中被粉碎。溶剂将约几微米的金属氧化物粘在载体表面上。通过在含氢的气氛中加热来还原金属氧化物。还原气体和目标金属接触。碳簇是由吸附的残留有机物提供的碳原子形成的。在真空中加热溶剂或石墨。例如,将直径为20-400nm的氧化铝粉末与直径为几μm的氧化钨粉末和醇混合。粉碎后,将所得的具有吸留的醇的钨掺杂氧化铝粉末4放入石墨容器1中,将容器1放置在碳纤维容器3中,并在吹入氢气的同时用碳加热器2加热粉末4。气态Ar

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号