PROBLEM TO BE SOLVED: To provide a dielectric ceramic composition from which a laminated ceramic capacitor having excellent dielectric characteristics while satisfying X7R characteristics and further having little deviation in the dielectric characteristics and good reliability can be obtained, and to provide a method for manufacturing the laminated ceramic capacitor by using the above composition.;SOLUTION: The laminated ceramic capacitor is composed of dielectric layers (2), inner electrode layers (3) formed in the dielectric layers by alternately laminating with the dielectric layers, and external electrodes (4) electrically connected to the inner electrode layers (3) and the dielectric layers and formed on the both ends of the dielectric layers. The dielectric layers (2) contain 0.5 to 4 mol MgO, 0.01 to 0.5 mol MnO, 0.1 to 2 mol BaO, 0.1 to 2 mol CaO and 1 to 4 mol SiO2 to 100 mol BaCaxTiO3 (0.001≤x≤0.02) and further contain at least one component selected from the group consisting of Y2O3, Dy2O3, Ho2O3 and Er2O3 by 0.1 to 3 mol.;COPYRIGHT: (C)2002,JPO
机译:解决的问题:提供一种介电陶瓷组合物,从该介电陶瓷组合物可以得到具有优异的介电特性同时满足X7R特性并且还具有极小的介电特性偏差和良好的可靠性的叠层陶瓷电容器,并且提供了用于制造该叠层陶瓷的方法解决方案:叠层陶瓷电容器由介电层(2),通过与介电层交替层压而形成在介电层中的内部电极层(3)和电气外部电极(4)组成连接至内部电极层(3)和介电层并形成在介电层的两端。介电层(2)包含0.5至4摩尔的MgO,0.01至0.5摩尔的MnO,0.1至2摩尔的BaO,0.1至2摩尔的CaO和1至4摩尔的SiO 2至100摩尔的BaCaxTiO 3(0.001& x≤ 0.02),并且进一步含有至少0.1至3摩尔的选自Y2O3,Dy2O3,Ho2O3和Er2O3的一种组分;版权:(C)2002,JPO

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号