The starting material is lateritic ore which contains nickeloxide and/or cobalt oxide. From water and comminuted ore, ofwhich at least 80 wt-% have grain sizes of not more than 0.5mm, a pumpable suspension is formed. The ore-containing sus-pension is passed through an indirectly heated preheatingtube, the suspension being heated to 150 to 250°C. The heatedsuspension is passed through a mixing line in which an acidin a minimum amount of 10 kg per 100 kg ore, calculated anhy-drous, is admixed to the suspension, and the acid-containingsuspension is passed through a dwell time tube in which thedwell time of the suspension is at least 0.1 minutes. Pref-erably, sulfuric acid is introduced into the mixing line.
机译:起始原料是含镍的红土矿石。氧化物和/或氧化钴。从水和粉碎的矿石中至少80 wt%的晶粒度不超过0.5mm,形成可泵送的悬架。含矿物质养老金通过间接加热的预热传递管,将悬浮液加热到150至250°C。加热悬浮液通过混合线,其中酸每100千克矿石最少10千克,计算得出的将Drous,混入悬浮液中,并将含酸悬浮液通过停留时间管,其中悬浮液的停留时间至少为0.1分钟。首选适当地,将硫酸引入混合管线。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号