首页> 外国专利> PROCESS OF LEACHING A LATERITIC ORE FOR PREPARING METAL EXTRACTION

PROCESS OF LEACHING A LATERITIC ORE FOR PREPARING METAL EXTRACTION

机译:浸出法制取金属矿石的方法

摘要

THE STARTING MATERIAL IS LATERITIC ORE HIGH CONTAINS NICKEL OXIDE AND/OR COBALT OXIDE. FROM WATER AND COMMINUTED ORE, OF WHICH AT LEAST 80-WTHAVE GRAIN SIZES OF NOT MORE THAN 0.5 NM, A PUMPABLE SUSPENSION IS FORMED. THE ORE-CONTAINING SUSPENSION IS PASSED THROUGH AN INDIRECTLY HEATED PREHEATING TUBE, THE SUSPENSION BEING HEATED TO 150 TO 250°C. THE HEATED PREHEATING TUBE, THE SUSPENSION IS PASSED THROUGH A MIXING LINE IN WHICH AN ACID IN A MINIMUM AMOUNT OF 10KG PER 100KG ORE, CALCULATED ANHYDROUS, IS ADMIXED TO THE SUSPENSION AND THE ACID-CONTAINING SUSPENSION IS PASSED THROUGH AD WELL TIME TUBE IN WHICH THE DWELL TIME OF THE SUSPENSION IS AT LEAST 0.1 MINUTES. PREFERABLY, SULFURIC ACID IS INTRODUCED INTO THE MIXING LIUNE.@@FIGURE 1
机译:起始材料是含铅的矿石或高含量的氧化镍和/或钴氧化物。在至少80瓦粒度不超过0.5海里的水和矿渣中,形成了可泵送的悬浮液。含矿悬浮液通过不加热的预热管通过,悬浮液加热到150至250°C。加热的预热管,悬浮液通过混合线通过,其中酸的最低含量为每100千克每公斤10千克以上,计算为无水,并与悬浮液混合,并在整个过程中输入含酸的悬浮液暂停的停留时间至少为0.1分钟。优选地,将硫酸引入到混合柳树中。@@图1

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号