PURPOSE: A method for cross-linking a high density polyethylene by using the plasma reaction and a latent heat regenerating material prepared by using the method are provided, to obtain a high density polyethylene with a low surface charge which stores heat by the form of slurry. CONSTITUTION: The method comprises the steps of charging a high density polyethylene with flowing a carrier gas into a plasma reactor; fluidizing the high density polyethylene slurry by stirring it with a Teflon-coated magnetic bar to cross-link the high density polyethylene; and introducing fluorine from Teflon to modify the surface. Preferably the cross-linking process is carried out in the condition of an RF power of 30-300 W, a pressure of 0-350 mTorr, a treatment time of 30 sec to 120 min, and a rotation velocity of a magnetic bar of 50-1,000 rpm. The carrier gas is preferably argon. The plasma electron energy of a reactor is 0.1-10 and the electron density is 10¬9-10¬12 cm¬-3.
机译:目的:提供一种通过等离子体反应使高密度聚乙烯交联的方法,以及使用该方法制备的潜热再生材料,以获得具有低表面电荷的高密度聚乙烯,该低表面电荷通过浆料的形式储存热量。组成:该方法包括以下步骤:在载气流入等离子反应器的过程中装入高密度聚乙烯;通过用涂有特氟龙的磁棒搅拌使高密度聚乙烯浆液流化以使高密度聚乙烯交联;并从特氟隆引入氟来改性表面。优选地,在RF功率为30-300W,压力为0-350mTorr,处理时间为30秒至120min,磁棒的旋转速度为50的条件下进行交联过程。 -1,000 rpm。载气优选是氩气。反应器的等离子体电子能为0.1-10,电子密度为10-9-10-12 cm--3。

著录项

  • 公开/公告号KR20020006979A

    专利类型

  • 公开/公告日2002-01-26

    原文格式PDF

  • 申请/专利权人 CHUNGNAM NATIONAL UNIVERSITY;

    申请/专利号KR20000040610

  • 发明设计人 CHOI HO SEOK;KIM JAE U;

    申请日2000-07-14

  • 分类号C08J3/24;

  • 国家 KR

  • 入库时间 2022-08-22 00:31:40

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号