首页> 外国专利> METHOD FOR MANUFACTURING POROUS CERAMIC WATER PURIFICATION FILTER USING SILVER CLUSTER IMPREGNATED ZEOLITE AND OYSTER SHELL

METHOD FOR MANUFACTURING POROUS CERAMIC WATER PURIFICATION FILTER USING SILVER CLUSTER IMPREGNATED ZEOLITE AND OYSTER SHELL

机译:银团浸渍沸石和牡蛎壳制造多孔陶瓷净水滤池的方法

摘要

PURPOSE: A method for manufacturing a porous ceramic water purification filter using silver cluster impregnated zeolite and oyster shell is provided to develop a ceramic water purification filter for filtering heavy metals and harmful organic compound and sterilizing bacteria as preserving natural water as it is. CONSTITUTION: The method for manufacturing a porous ceramic water purification filter using silver cluster impregnated zeolite and oyster shell comprises the processes of dehydrating the ion exchanged zeolite at 500 deg.C under the oxygen current after ion exchanging silver (Ag) onto zeolite; forming the mixture in a cylindrical shape by mixing diatomaceous earth and clay or bentonite with the oyster shell powder in a certain ratio after calcining oyster shell at 1000 deg.C and milling the calcined oyster shell into powder; and manufacturing a ceramic water purification filter having a high ceramic porosity after heat treating the resulting material at a relatively low temperature of 700 to 900 deg.C, wherein the ceramic water purification filter comprises the processes of mixing 40 to 60 wt.% of diatomaceous earth having particle size of 100 m or less, 10 to 30 wt.% of stabilized silver cluster that is prepared by dehydrating zeolite onto which silver (Ag) having excellent ion exchange capability is ion exchanged under the oxygen current, 3 to 5 wt.% of oyster shell powder, and 10 to 40 wt.% of viscous yellow soil or bentonite; and calcining the mixture at a temperature of 700 to 900 deg.C.
机译:目的:提供一种使用银团浸渍的沸石和牡蛎壳制造多孔陶瓷净水过滤器的方法,以开发一种陶瓷净水过滤器,用于过滤重金属和有害有机化合物以及对细菌进行杀菌以保持原样的天然水。组成:一种用银团浸渍的沸石和牡蛎壳制造多孔陶瓷净水过滤器的方法,包括将离子交换银(Ag)离子交换到沸石上后,在氧气流下于500℃对离子交换沸石进行脱水的过程。将牡蛎壳在1000℃下煅烧后,将硅藻土,粘土或膨润土与牡蛎壳粉按一定比例混合,制成圆柱状混合物。以及在700至900℃的相对较低的温度下对所得材料进行热处理之后,制造具有高陶瓷孔隙率的陶瓷净水过滤器,其中该陶瓷净水过滤器包括混合40至60重量%的硅藻土的过程粒径为100 m以下的10%至30 wt%的稳定化银簇,该簇是通过将沸石脱水而制得的,该沸石在氧气流下通过离子交换将具有优异离子交换能力的银(Ag)3至5 wt%。 %的牡蛎壳粉,和10%至40%重量的粘性黄土或膨润土;并在700至900℃的温度下煅烧混合物。

著录项

  • 公开/公告号KR20020075156A

    专利类型

  • 公开/公告日2002-10-04

    原文格式PDF

  • 申请/专利权人 LEE SEOK HEE;

    申请/专利号KR20010016096

  • 发明设计人 LEE SEOK HEE;MUN SEONG BAE;OH CHA JAE;

    申请日2001-03-23

  • 分类号B01D39/20;

  • 国家 KR