ONE-PACK MOISTURE-CURING URETHANE RESIN-BASED LEVELING MATERIAL AND METHOD FOR LEVELING USING THE SAME

机译:基于单包保湿型聚氨酯树脂的铺层材料和使用该材料的铺层方法

摘要

PROBLEM TO BE SOLVED: To obtain a one-pack moisture-curing urethane-based leveling material by which a conventional leveling method is rationalized.;SOLUTION: The leveling material comprises an isocyanate-terminal urethane prepolymer, a nonhollow filler and a hollow filler having a particle diameter larger than that of the nonhollow filler. The isocyanate-terminal urethane prepolymer is obtained by reacting a polyol with an isocyanate compound. A polyol mixed with 25-100 mass % of a polyoxypropylene polyol having ≤0.035 milliequivalent/g unsaturation degree and 1,500-20,000 number-average molecular weight (Mn) is used as the polyol. The isocyanate content of the isocyanate- terminal urethane prepolymer is preferably 1-10%. Preferably the average particle diameter of the nonhollow filler is 0.01-8 μm and the average particle diameter of the hollow filler is 20-200 μm.;COPYRIGHT: (C)2003,JPO
机译:解决的问题:获得一种使传统流平方法合理化的一包湿气固化型聚氨酯基流平材料;解决方案:该流平材料包括异氰酸酯端基氨基甲酸酯预聚物,一种非空心填料和一种具有粒径大于非空心填料的粒径。通过使多元醇与异氰酸酯化合物反应获得异氰酸酯末端氨基甲酸酯预聚物。将多元醇与25-100质量%的具有≤0.035毫当量/ g的不饱和度和1,500-20,000数均分子量(Mn)的聚氧化丙烯多元醇混合。异氰酸酯末端氨基甲酸酯预聚物的异氰酸酯含量优选为1-10%。非空心填料的平均粒径优选为0.01-8μm,空心填料的平均粒径为20-200μm。COPYRIGHT:(C)2003,JPO

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号