首页> 外国专利> Method of raising the yield strength of cold-formed profile steel

Method of raising the yield strength of cold-formed profile steel

机译:提高冷弯型钢屈服强度的方法

摘要

PCT No. PCT/AU95/00378 Sec. 371 Date Dec. 26, 1996 Sec. 102(e) Date Dec. 26, 1996 PCT Filed Jun. 27, 1995 PCT Pub. No. WO96/00305 PCT Pub. Date Jan. 4, 1996Yield strength of a cold rolled steel section is increased and controlled by performing a predetermined amount of strain by way of cold working in an in-line roll forming process followed by a controlled amount of strain aging wherein the temperature of the steel section is elevated to a point below 500 DEG C. and held at an elevated temperature for a time up to 30 seconds. The heating typically takes place by induction heaters (16) and the time aging may be provided in an in-line galvanizing bath (17) before cooling the steel in a quench bath (18). The effect is further enhanced by further cold working and the consequent additional strain in forming rolls (19). For a given steel composition the degree of yield enhancement can be controlled by the temperature and tie parameters and also by the degree of initial roll forming in shaping rolls (10).
机译:PCT号PCT / AU95 / 00378第371日期1996年12月26日102(e)日期,1996年12月26日PCT,1995年6月27日提交,PCT Pub。 WO96 / 00305 PCT公开号日期1996年1月4日,通过在线轧制过程中进行冷加工,执行预定量的应变,然后控制量的应变时效,其中控制温度的变化来提高和控制冷轧钢件的屈服强度。将钢段升高到低于500℃的点,并在升高的温度下保持长达30秒的时间。通常通过感应加热器(16)进行加热,并且可以在在线镀锌浴(17)中提供时效,然后在淬火浴(18)中冷却钢。通过进一步的冷加工以及随之而来的成形辊(19)的额外应变,进一步提高了效果。对于给定的钢成分,屈服增强的程度可以通过温度和连接参数以及成型辊(10)中初始轧制的程度来控制。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号