PROBLEM TO BE SOLVED: To prevent generation of defect in external appearance by arranging a difference in levels to a hem bending part of thick plate side and coinciding a hem bending curvature of thick plate side to a hem bending part of thin plate side so as to eliminate unevenness of an clearance, etc., whenever there is a difference in plate thicknesses. ;SOLUTION: At the side of a thin plate panel Pi2 of inner panel Pi, pressing is executed with using a hem pad 2 arranged with a normal flat plane shaped pressing face, the curvature radius R2 of hem bending part is turned to t2/2+t3. On the other hand, at the side of a thick plate panel Pi1, because a difference in level part 2a corresponding to a plate thickness difference t1-t2 between the thick plate panel Pi1 and thin plate panel Pi2 is formed t the pressing face of a hem pad 2, the curvature radius R1 of hem bending part, resulting from that a tip part is crushed by the difference in levels part 2a of hem pad 2 to form a difference in levels D, is turned to t2/2+t3, that is equal to the curvature radius R2 of thin plate side. Thus, unevenness of clearance and incontinuousness of hemming part are eliminated.;COPYRIGHT: (C)1998,JPO
机译:解决的问题:通过在厚板侧的下摆弯曲部分上设置高度差,并且使厚板侧的下摆弯曲曲率与薄板侧的下摆弯曲部分重合,以防止外观缺陷的产生。只要板厚不同,就可以消除间隙等的不均。 ;解决方案:在内部面板Pi的薄板面板Pi2的一侧,通过使用配置有正常平面形状的按压面的下摆垫2进行按压,下摆弯曲部的曲率半径R2变为t 2 / 2 + t 3 。另一方面,在厚板面板Pi1侧,因为与厚板之间的板厚差t 1 -t 2 相对应的水平部2a的差。在下摆垫2的按压面,下摆弯曲部的曲率半径R1形成有板面板Pi1,薄板面板Pi2,这是由于下端部因下摆垫2的高度差2a而压碎而形成的。水平差D变为t 2 / 2 + t 3 ,等于薄板侧的曲率半径R2。因此,消除了间隙的不均匀性和包边部分的不连续性。;版权所有:(C)1998,日本特许厅

著录项

  • 公开/公告号JP3644466B2

    专利类型

  • 公开/公告日2005-04-27

    原文格式PDF

  • 申请/专利权人 日産自動車株式会社;

    申请/专利号JP19960191106

  • 发明设计人 内 島 宏 明;

    申请日1996-07-19

  • 分类号B21D39/02;B21D19/08;

  • 国家 JP

  • 入库时间 2022-08-21 22:26:40

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号