Precipitation hardened Co-Ni based heat-resistant alloy and production method therefor

机译:沉淀硬化的Co-Ni基耐热合金及其生产方法

摘要

A precipitation hardened Co-Ni based heat-resistant alloy is composed of, all by weight, not more than 0.05% of C; not more than 0.5% of Si; not more than 1.0% of Mn; 25 to 45% of Ni; 13 to 22% of Cr; 10 to 18% of Mo or 10 to 18% of Mo + 1/2W; 0.1 to 5.0% of Nb; 0.1 to 5.0% of Fe; and further at least one kind of 0.007 to 0.10% of REM; 0.001 to 0.010% of B; 0.0007 to 0.010% of Mg and 0.001 to 0.20% of Zr; the balance of substantially Co and inevitable impurities, and Co3Mo or Co7Mo6 is precipitated in boundaries between a fine twin structure and a parent phase.
机译:沉淀硬化的Co-Ni基耐热合金全部按重量计由不超过0.05%的C组成;不超过Si的0.5%;不超过锰的1.0%; Ni的25%至45%; Cr的13%至22%; Mo的10%至18%或Mo的10%至18%+ 1 / 2W; Nb的0.1至5.0%;铁的0.1至5.0%;并且还具有0.007〜0.10%的REM中的至少一种。 B的0.001至0.010%;镁为0.0007至0.010%,锆为0.001至0.20%;基本上是Co和不可避免的杂质的平衡,而Co3Mo或Co7Mo6则沉淀在精细孪晶结构和母相之间的边界中。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号