The present invention, transfer heat to be supported, and occurs while reducing the frictional resistance of the guide such as to be moved to a rotated shaft and the horizontal to facilitate the base metal according to the production method of the white metal wires used for welding growth of metal bearing the white metal wire to a method of producing an extrusion which is used to form the metal bearing of the arc welding.; According to the invention, the first step by dissolving the white metal casting a billet, the billet 1.1 ~ 1.2 times than the final diameter of the white metal wire while maintaining the preheating temperature after 2-4 hours pre-heated to a temperature of 120 ~ 140 ℃ the production method of the white metal wires used for the second step, the extruded wire for performing the extrusion welding growth of metal bearing consisting of a third step in the diameter of the end of the fresh white metal wire is provided.
机译:根据用于焊接的白色金属线的制造方法,本发明传递热量以被支撑,并且在减小例如被移动到旋转的轴和水平方向的引导件的摩擦阻力的同时发生,以利于母材。将带有白色金属丝的金属生长到生产挤压件的方法,该挤压件用于形成电弧焊的金属轴承。根据本发明,第一步是通过溶解白色金属铸造的坯料,该坯料为白色金属丝的最终直径的1.1〜1.2倍,同时在预热2-4小时后保持120℃的预热温度至120℃的温度提供约140℃的第二步骤中使用的白色金属线的制造方法,提供一种用于进行金属轴承的挤压焊接生长的挤压线,该挤压线包括第三步,其在新鲜的白色金属线的端部的直径中。

著录项

  • 公开/公告号KR20050092686A

    专利类型

  • 公开/公告日2005-09-22

    原文格式PDF

  • 申请/专利权人 SHINWOO METAL INDUSTRIAL CO. LTD.;

    申请/专利号KR20050080793

  • 发明设计人 SIN JI KEUN;

    申请日2005-08-31

  • 分类号B23K35/40;

  • 国家 KR

  • 入库时间 2022-08-21 22:04:35

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号