HIGH-STRENGTH/HIGH-CONDUCTIVITY COPPER ALLOY HAVING EXCELLENT WORKABILITY, AND COPPER ALLOY MEMBER USING THE SAME

机译:高强度/高导电性的铜合金具有出色的可加工性,并且铜合金使用相同的元件

摘要

PROBLEM TO BE SOLVED: To provide a new copper alloy material in which strength, bending workability, press blanking properties, stress relaxation resistance and the anisotropy thereof are simultaneously improved to high levels while maintaining its high conductivity level of ≥70%IACS.;SOLUTION: The copper alloy has a composition comprising, by mass, 0.1 to 0.3% Fe, 0.05 to 0.3% Ni, 0.04 to 0.2% P and 0.03 to 0.15% Sn, and in which the total content of elements other than Cu and the above elements is ≤0.1%, and the balance Cu, and has a structure where, regarding crystal grains in the cross-section parallel to the rolling direction and the sheet thickness direction, the average aspect ratio (major axis/minor axis) A is ≥10, and the ratio between the maximum value Amax and the minimum value Amin of the aspect ratio, Amax/Amin is 1.0 to 3.0.;COPYRIGHT: (C)2007,JPO&INPIT
机译:解决的问题:提供一种新的铜合金材料,其中强度,弯曲加工性,冲压冲裁性能,抗应力松弛性及其各向异性同时提高到高水平,同时保持其高导电率水平为70%IACS。 SOLUTION:铜合金的成分为质量百分比为0.1到0.3%的铁,0.05到0.3%的镍,0.04到0.2%的P和0.03到0.15%的Sn,其中除Cu和上述元素为0.1%,余量为Cu,具有平行于轧制方向和板厚方向的截面的晶粒的平均长径比(长轴/短轴)A的结构。为≥ 10,并且宽高比的最大值A max 与最小值A min 之比A max / A min 是1.0到3.0 。;版权所有:(C)2007,JPO&INPIT

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号