PPROBLEM TO BE SOLVED: To provide a high fluidity titanium oxide suitable for obtaining toner for electrostatic latent image development having good fluidity, ensuring small environmental variation of charging performance and stably giving a high sharpness image, and to provide a toner for electrostatic latent image development having the above properties by adding the high fluidity titanium oxide as an external additive. PSOLUTION: The high fluidity titanium oxide is obtained by dry-mixing a titanium oxide having an average primary particle diameter of 5-100 nm hydrophobed with an organic substance and silica having an average primary particle diameter of 5-40 nm manufactured by a gas phase method in a silica to titanium oxide ratio of 0.5-20 mass%. The toner for electrostatic latent image development is obtained by adding the high fluidity titanium oxide as an external additive. PCOPYRIGHT: (C)2006,JPO&NCIPI
机译:

要解决的问题:提供一种高流动性的氧化钛,该氧化钛适于获得具有良好流动性的静电潜像显影用调色剂,确保带电性能的环境变化小并稳定地提供高清晰度图像,并提供用于静电的调色剂通过添加高流动性的氧化钛作为外部添加剂,具有上述性质的潜像显影。

解决方案:高流动性的二氧化钛是通过将疏水化的平均一次粒径为5-100 nm的氧化钛与有机物和由以下方法制造的平均一次粒径为5-40 nm的二氧化硅干混而成的:气相法中二氧化硅与氧化钛的比例为0.5-20质量%。通过添加高流动性的氧化钛作为外部添加剂来获得用于静电潜像显影的调色剂。

版权:(C)2006,JPO&NCIPI

著录项

  • 公开/公告号JP2006195025A

    专利类型

  • 公开/公告日2006-07-27

    原文格式PDF

  • 申请/专利权人 TAYCA CORP;

    申请/专利号JP20050004705

  • 发明设计人 ASADA YUKINOBU;

    申请日2005-01-12

  • 分类号G03G9/08;

  • 国家 JP

  • 入库时间 2022-08-21 21:55:37

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号