首页> 外国专利> Production manner of the unpolished rice powder, comminution the raw materials unpolished rice which is dried with dry process and the said dry process which dry the raw materials unpolished rice which the moist heat treatment is done

Production manner of the unpolished rice powder, comminution the raw materials unpolished rice which is dried with dry process and the said dry process which dry the raw materials unpolished rice which the moist heat treatment is done

机译:粗米粉的制造方式,将通过干燥工序干燥的原料粗米粉粉碎,以及将进行了湿热处理的原料粗米粉干燥的上述干燥工序进行粉碎。

摘要

PROBLEM TO BE SOLVED: To modify a starch so as hardly to be gelatinized in a proper range and to modify the starch so as to reduce the viscosity of a gelatinized solution in a proper range even if the starch is gelatinized. SOLUTION: In this method for producing unpolished rice flour comprising a wet- heat treatment process for subjecting raw material unpolished rice as it is to a wet-heat treatment, a drying process for drying the raw material unpolished rice subjected to the wet-heat treatment by the wet-heat treatment process and a flouring process for flouring the raw material unpolished rice dried by the drying process to give unpolished rice flour, the wet-heat treatment is carried out so that at least two of (1) a relative peak intensity in a diffraction peak 3b (angle of diffraction 2θ is 15 deg) derived from the starch is 0.012-0.023, (2) a relative peak intensity in a diffraction peak 4a-4b (angle of diffraction 2 θ is 17-18 deg) is 0.030-0.070 and (3) a relative peak intensity in a diffraction peak 6a (angle of diffraction 2θ is 23 deg) is 0.030-0.060 are exhibited when a relative peak intensity of X-ray diffraction is measured by an X-ray diffraction apparatus under a fixed condition.
机译:解决的问题:即使淀粉被糊化,也难以在适当范围内使淀粉糊化而对淀粉进行改性,并且在适当范围内将淀粉糊化溶液的粘度降低至适当范围内。解决方案:在这种生产糙米粉的方法中,包括对原糙米进行湿热处理的湿热处理工艺,以及对经过湿热处理的原料糙米进行干燥的干燥工艺。通过湿热处理工序和用于将通过干燥工序干燥的原料糙米进行面粉制粉而得到糙米粉的撒粉工序,进行湿热处理,使得(1)中的至少两个具有相对峰值强度。由淀粉衍生的衍射峰3b(衍射角2θ为15度)在0.012-0.023,(2)在衍射峰4a-4b中的相对峰强度(衍射角2θ为17-18度)。 )为0.030〜0.070,(3)通过X射线衍射法测定X射线衍射的相对峰强度时,衍射峰6a(衍射角2θ为23度)的相对峰强度为0.030〜0.060。固定下的射线衍射仪健康)状况。

著录项

  • 公开/公告号JP3780154B2

    专利类型

  • 公开/公告日2006-05-31

    原文格式PDF

  • 申请/专利权人 岩手県パン工業組合;

    申请/专利号JP20000235853

  • 发明设计人 三浦 靖;

    申请日2000-08-03

  • 分类号A23L1/10;A21D2/36;A21D13/00;

  • 国家 JP

  • 入库时间 2022-08-21 21:49:56