首页> 外国专利> Titanium-made cathode electrode for producing electrolytic copper foil, rotary cathode drum using the titanium-made cathode electrode, method of producing titanium material using titanium-made cathode electrode and method of correcting/working titanium material for titanium-made cathode electrode

Titanium-made cathode electrode for producing electrolytic copper foil, rotary cathode drum using the titanium-made cathode electrode, method of producing titanium material using titanium-made cathode electrode and method of correcting/working titanium material for titanium-made cathode electrode

机译:用于制造电解铜箔的钛制阴极电极,使用该钛制阴极电极的旋转阴极鼓,使用钛制阴极电极制造钛材料的方法以及校正/加工用于钛制阴极电极的钛材料的方法

摘要

The purpose is to provide a cathode electrode for manufacturing an electrodeposited copper foil which is possible to be continuously and stably usable for a long duration of 3000 hours or longer to subsequently lessen the frequency of maintenance work execution as low as possible and to contribute to lower the running cost of the electrodeposited copper foil manufacture. As the means for achieving the purpose, a cathode electrode made of a titanium material is employed for obtaining an electrodeposited copper foil using an electrolytic copper solution and the titanium material having 7.0 or higher crystal grain size number and 35 ppm or lower initial hydrogen content is used for manufacturing the cathode electrode for manufacturing an electrodeposited copper foil. Further, also provided is a manufacturing method of the titanium material to be employed for the cathode electrode made of a titanium material.
机译:目的是提供一种用于制造电沉积铜箔的阴极电极,该阴极电极可连续稳定地使用3000小时或更长时间,从而尽可能地减少维护工作的执行频率并有助于降低成本。电沉积铜箔生产的运行成本。作为实现该目的的手段,使用由钛材料制成的阴极电极来使用电解铜溶液获得电沉积铜箔,并且该钛材料具有7.0以上的晶粒尺寸数和35ppm以下的初始氢含量。用于制造用于制造电沉积铜箔的阴极。此外,还提供了用于由钛材料制成的阴极电极的钛材料的制造方法。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号