首页> 外国专利> Method of fabricating ZnO nanowires and ZnO nanowires fabricated from the same

Method of fabricating ZnO nanowires and ZnO nanowires fabricated from the same

机译:ZnO纳米线的制造方法以及由其制备的ZnO纳米线

摘要

PURPOSE: Provided is a simple method for preparing ZnO nanowires by oxidizing ZnO particles formed through thermal deposition in the air unlike the conventional method under vacuum or gas atmosphere. CONSTITUTION: The ZnO nanowires or ZnO particles comprising Zn nanowires on the surface of Zn metal are prepared by forming Zn particles through thermal deposition process, depositing Zn metal(37) on a sapphire substrate(29), and then oxidizing Zn particles at 900deg.C or higher at least 10min under air atmosphere. The resultant nanowires have zinc-oxygen having a ratio Zn/O of 1 to 1, and large diameter and long length as time and temperature for oxidation get higher and longer.
机译:目的:提供一种简单的方法,通过氧化在空气中通过热沉积形成的ZnO颗粒来制备ZnO纳米线,这与常规方法在真空或气体气氛下不同。组成:ZnO纳米线或在Zn金属表面上包含Zn纳米线的ZnO颗粒是通过热沉积工艺形成Zn颗粒,在蓝宝石衬底(29)上沉积Zn金属(37),然后在900度氧化Zn颗粒而制备的。空气中至少10分钟或更高。所得的纳米线具有Zn / O比为1:1的锌-氧,并且随着氧化的时间和温度变得越来越高,直径大且长度长。

著录项

  • 公开/公告号KR100614130B1

    专利类型

  • 公开/公告日2006-08-22

    原文格式PDF

  • 申请/专利权人

    申请/专利号KR20030044971

  • 申请日2003-07-03

  • 分类号B82B3;

  • 国家 KR

  • 入库时间 2022-08-21 21:23:12

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号